Aug 11, 2022 Leave a message

Control of printed board quality and components before wave soldering

1. Circuit board pad design

1) When designing the plug-in component pads, the size of the pads should be designed appropriately. If the pad is too large, the solder spreading area is large, and the formed solder joint is not full, while the surface tension of the copper foil of the smaller pad is too small, and the formed solder joint is a non-wetting solder joint. The matching gap between the aperture and the lead of the component is too large, and it is easy to solder. When the aperture is 0.05 - 0.2mm wider than the lead, and the diameter of the pad is 2 - 2.5 times the aperture, it is an ideal condition for welding.

2) When designing the SMD component pads, the following points should be considered:

a. In order to remove the "shadow effect" as much as possible, the soldering end or pin of the SMD should be facing the direction of the tin flow, so as to facilitate the contact with the tin flow and reduce the virtual soldering and missing soldering.

b. Wave soldering is not suitable for fine-pitch QFO, PLCC, BGA and small-pitch SOP device soldering, that is to say, try not to arrange such components on the side to be wave soldered.

c. Smaller components should not be arranged after larger components, so as to prevent the larger components from hindering the solder flow from contacting the pads of smaller components and causing leakage soldering.

2, PCB circuit board flatness control

Wave soldering has high requirements on the flatness of the printed board. Generally, the warpage is required to be less than 0.5mm, and if it is greater than 0.5mm, it needs to be flattened. In particular, the thickness of some printed boards is only about 1.5mm, and the warpage requirements are higher, otherwise the welding quality cannot be guaranteed.

3. Properly preserve the printed board and components, and try to shorten the storage period. During welding, copper foil and component leads without dust, grease and oxide are conducive to the formation of qualified solder joints. Therefore, the printed board and components should be stored in a dry, dry place. In a clean environment, and keep the storage period as short as possible. For printed boards that have been placed for a long time, the surface is generally cleaned, which can improve solderability and reduce virtual soldering and bridging. For component pins with a certain degree of surface oxidation, the surface oxide layer should be removed first.


Send Inquiry

whatsapp

teams

E-mail

Inquiry