How long is the reflow soldering preheat time?

It depends on the part with the largest heat capacity on the PCB, the PCB area, the thickness of the PCB, and the performance of the solder paste used. Generally, the time in the preheating period of 80-160℃ is 60-120sec, which effectively removes the volatile solvent in the solder paste, reduces the thermal shock to the components, and at the same time fully activates the flux and makes the temperature difference smaller. . • Rate of temperature rise in the preheating stage: For the heating stage, a slow rate of rise in the temperature range between room temperature and melting point is expected to reduce most defects. For the optimal curve, a slow rise rate of 0.5 to 1 °C/sec is recommended, and for the traditional curve, it is better to increase the temperature below 3 to 4 °C/sec.